Duplex Stainless Steel

June 21, 2016  
Foundry Duplex Stainless Steel

Duplex stainless steel is two tiers of toughness composed of microscopic grains of ferritic and austenitic stainless steel, layered like your mother-in-law’s coffee cake, and nearly as hard to chew. It boasts a greater strength than either type of steel individually, and it’s very resistant to stress corrosion cracking.  It… Read more »